On 20 November 2026 the US Federal Aviation Administration (FAA) published a final airworthiness directive for all Airbus A330-841 and A330-941 airplanes (AD 2026-23-01, issued 6 November 2026). It followed reports of cracks on the discharge outlet of engine fire extinguisher bottles with part number 34500063-11.
What the source reports
The FAA cites an EASA directive of 12 February 2025. EASA states that investigations found the heat treatment applied in production makes these parts susceptible to stress corrosion cracking. It found the performance of the engine fire extinguishing system largely unaffected, though the rate of findings qualified the condition as potentially unsafe. The FAA adds that cracking could get worse over time and eventually let the extinguisher agent leak.
The directive requires modification of the affected bottles, which means replacing the discharge outlet, and bars installing the part. Commenters asked for alternative materials and for a shorter compliance time. The FAA refused both and kept 30 months. It estimates 35 airplanes on the US register, at 11 work-hours each.
What it means for asset owners
In our view, stress corrosion cracking depends on three things together: a susceptible condition of the metal, tensile stress and a corrosive environment. Here the first one came from the production route. A specification that names the alloy but not its heat treatment leaves that variable unchecked.
Source: US Federal Aviation Administration, Federal Register, 20 November 2026.